Details
*Similar Grade
GB JIS Trademark UNS DIN NF ГОСТ BS
1J76 PC-2
PC-22 Mumetal
Round Permalloy 80
HyMu 80
HyMu 77 N14076 Mumetal
Vacoperm Mumetal
Permimphy 1 76НХД Mumetal M2, M2+
Supermumetal SM2
1J77 77НМД
1J79 Supermalloy
Square Permalloy 80
HyMu 80 Ⅱ
HyRa 80 N14080 Ultraperm 10
Ultraperm 200
Ultraperm 300
Ultraperm F80
Ultraperm 200TK
Ultraperm Z Permimphy 2
Permimphy 5
Permimphy 6
Permimphy C 79Н Supermumetal SM150, 250
Supermumetal SM300
1J80 80НХС
1J85 PC-80
PC-3 Super-permalloy
Wacumate
*Specification
GBn 198-88, ГОСТ 10994-1974, ГОСТ 10160-1975, ASTM A753-2008
*Product Forms
Pipe, Tube, Sheet, Strip, Plate, Round Bar, Flat Bar, Forgings, Hexagon, Wire
*Chemical Composition,%
Alloy C P S Si Mn Ni Cu Co Cr Fe
1J76 ≤0.03 ≤0.02 ≤0.02 0.15-0.30 0.30-0.60 75.0-76.5 4.80-5.20 - 1.80-2.20 Rest
1J77 ≤0.03 ≤0.02 ≤0.02 0.15-0.30 0.30-0.60 75.0-78.0 4.80-6.00 - - Rest
1J79 ≤0.03 ≤0.02 ≤0.02 0.30-0.50 0.60-1.10 78.5-80.0 ≤0.20 - - Rest
1J80 ≤0.03 ≤0.02 ≤0.02 1.10-1.50 0.60-1.10 79.0-81.5 ≤0.30 - 2.60-3.00 Rest
1J85 ≤0.03 ≤0.02 ≤0.02 0.15-0.30 0.30-0.60 79.0-81.0 ≤0.20 - - Rest
1.86 ≤0.03 ≤0.02 ≤0.02 ≤0.30 ≤1.00 80.5-81.5 - - - Rest
*AC Magnetic Properties of Soft Magnetic alloys with High Permeability and Fairly High Saturation Magnetic Induction
Alloy Type Thickness, mm Elastic permeability at different frequencies measured at the peak value of magnetic field intensity of 0.1 A/m, μm/mH˙m-1
60 Hz 400 Hz 1 kHz 10 kHz
1J79 Cold rolled strip 0.02 - - ≥14000(17.5) ≥10000(12.5)
0.05 - - ≥15040(18.8) ≥7520(9.4)
0.10 - ≥18000(22.5) ≥12000(15) -
0.20 - ≥10000(12.5) ≥6000(7.5) -
0.35 ≥25 ≥7040(8.8) - -
1J85 Cold rolled strip 0.02 - - ≥16000(20) ≥12000(15)
0.05 - - ≥25040(31.3) ≥9040(11.3)
0.10 - ≥25040(31.3) ≥20000(25) -
0.20 - ≥19040(23.8) ≥8000(10) -
0.35 ≥38 ≥10000(12.5) - -
*DC Magnetic Properties of Soft Magnetic alloys with High Permeability and Fairly High Saturation Magnetic Induction
Alloy Type Class Thickness, mm Permeability at a magnetic field intensity of 0.4 A/m, μ0.4/mH˙m-1 Maximum permeability μm/mH˙m-1 Coercive force (under saturation magnetic induction) Hc/A˙m-1 Saturation magnetic induction Bs/T
1J76 Cold rolled strip 0.02-0.04 ≥15040(18.8) ≥60000(75) ≤4.8 0.75
0.05-0.09 ≥18000(22.5) ≥100000(125) ≤3.2 0.75
0.10-0.19 ≥20000(25) ≥140000(175) ≤2.8 0.75
0.20-0.50 ≥25040(31.3) ≥180000(225) ≤1.4 0.75
1J77 Cold rolled strip 0.05-0.09 ≥30000(37.5) ≥140000(175) ≤1.4 0.60
0.10-0.19 ≥40000(50) ≥180000(225) ≤2.0 0.60
0.20-0.34 ≥50000(62.5) ≥220000(275) ≤1.2 0.60
0.35-0.50 ≥60000(75) ≥250000(312.5) ≤1.0 0.60
1J79 Cold rolled strip Ⅰ 0.02-0.04 ≥16000(20) ≥90000(112.5) ≤4.0 0.75
0.05-0.09 ≥18000(22.5) ≥110000(137.5) ≤2.8 0.75
0.10-0.19 ≥20000(25) ≥130000(162.5) ≤2.0 0.75
0.20-0.34 ≥22400(28) ≥180000(225) ≤1.6 0.75
0.35-1.00 ≥24600(31) ≥200000(250) ≤1.2 0.75
1.10-2.50 ≥22400(28) ≥180000(225) ≤1.6 0.75
Ⅱ 0.02-0.04 ≥20000(25) ≥100000(125) ≤2.4 0.75
0.05-0.09 ≥20000(25) ≥120000(150) ≤1.6 0.75
0.10-0.19 ≥22400(28) ≥152000(190) ≤1.2 0.75
0.20-0.34 ≥24800(31) ≥200000(250) ≤1.2 0.75
0.35-1.00 ≥30400(38) ≥224000(280) ≤1.0 0.75
1.10-2.50 ≥24800(31) ≥184000(230) ≤1.2 0.75
Ⅲ 0.02-0.04 ≥24800(31) ≥152000(190) ≤1.6 0.73
0.05-0.09 ≥30400(38) ≥200000(250) ≤1.2 0.73
0.10-0.19 ≥30400(38) ≥200000(250) ≤1.2 0.73
0.20-0.34 ≥30400(38) ≥224000(280) ≤1.0 0.73
0.35- ≥35200(44) ≥248000(310) ≤1.0 0.73
Hot rolled flat 4.5-20.00 ≥20000(25) ≥100000(125) ≤2.4 0.75
Hot rolled rod 20.00-100.00 ≥20000(25) ≥100000(125) ≤2.4 0.75
1J80 Cold rolled strip Ⅰ 0.03-0.04 ≥18400(23) ≥75040(93.8) ≤4.0 0.65
0.05-0.09 ≥20000(25) ≥90000(112.5) ≤3.2 0.65
0.10-0.19 ≥22400(28) ≥120000(150) ≤2.4 0.65
0.20-0.34 ≥28000(35) ≥140000(175) ≤1.6 0.65
0.35-0.50 ≥35200(44) ≥160000(200) ≤1.2 0.65
0.50-1.00 ≥35040(43) ≥160000(200) ≤1.0 0.65
1.10-2.50 ≥24800(31) ≥152000(190) ≤1.2 0.65
Ⅱ 0.03-0.04 ≥22400(28) ≥100000(125) ≤3.2 0.63
0.05-0.09 ≥30400(38) ≥152000(190) ≤1.6 0.63
0.10-0.19 ≥32000(40) ≥160000(200) ≤1.2 0.63
0.20-0.34 ≥35200(44) ≥160000(200) ≤1.2 0.63
0.35-0.50 ≥35200(44) ≥200000(250) ≤1.0 0.63
Ⅲ 0.03-0.04 ≥30400(38) ≥120000(150) ≤1.6 0.63
0.05-0.09 ≥40000(50) ≥200000(250) ≤1.0 0.63
0.10-0.34 ≥44800(56) ≥200000(250) ≤1.0 0.63
0.35-0.50 ≥50400(63) ≥248000(310) ≤0.8 0.63
Hot rolled flat 4.50-20.00 ≥22000(27.5) ≥80000(100) ≤2.4 0.65
Hot rolled rod 20.00-100.00 ≥22000(27.5) ≥80000(100) ≤2.4 0.65
1J85 Cold rolled strip Ⅰ 0.03-0.04 ≥18000(22.5) ≥80000(100) ≤3.6 0.70
0.05-0.09 ≥28000(35) ≥110000(137.5) ≤2.4 0.70
0.10-0.19 ≥30000(37.5) ≥150000(187.5) ≤1.6 0.70
0.20-0.34 ≥40000(50) ≥180000(225) ≤1.2 0.70
0.35-1.00 ≥50000(62.5) ≥250000(312.5) ≤0.8 0.70
1.10-2.50 ≥40000(50) ≥150000(187.5) ≤1.2 0.70
Ⅱ 0.03-0.04 ≥30000(37.5) ≥110000(137.5) ≤2.4 0.70
0.05-0.09 ≥40000(50) ≥140000(175) ≤1.6 0.70
0.10-0.19 ≥50000(62.5) ≥180000(225) ≤1.2 0.70
0.20-0.34 ≥60000(75) ≥200000(250) ≤1.0 0.70
0.35- ≥55040(68.8) ≥260000(325) ≤0.7 0.70
Hot rolled flat 4.50-20.00 ≥30000(37.5) ≥100000(125) ≤1.6 0.70
Hot rolled rod 20.00-100.00 ≥30000(37.5) ≥100000(125) ≤1.6 0.70
1J86 Cold rolled strip 0.03-0.04 ≥30000(37.5) ≥110000(137.5) ≤2.4 0.60
0.05-0.09 ≥40000(50) ≥150000(187.5) ≤1.4 0.60
0.10-0.19 ≥50000(62.5) ≥180000(225) ≤1.2 0.60
0.20-0.34 ≥60000(75) ≥220000(275) ≤0.7 0.60
0.35-1.00 ≥50000(62.5) ≥200000(250) ≤1.2 0.60
Note: Saturation magnetic induction Bs is measured at a magnetic field intensity of 800 A/m.
*Feature
High or much higher initial permeability and maximum permeability, extremely low coercive force and fairly low saturation magnetic induction.
*Application
High sensitive and small power transformers used in a weak magnetic field, magnetic amplifiers, relays reactors, magnetic heads of magnetic recording equipments, magnetic shielding, a variety of strip wound cores, and lamination cores, etcs.